The technical difference between C11000 and C10100 lies in their refining process, specifically the oxygen content and chemical purity. C11000, also known as Electrolytic Tough Pitch (ETP) copper, contains 99.90% minimum copper and 0.02% to 0.04% oxygen. In contrast, C10100, or Oxygen-Free Electronic (OFE) copper, is a high-purity grade with 99.99% minimum copper and virtually no oxygen (less than 5 ppm). For a comprehensive look at available forms, visit our C11000 product overview. While C11000 is the standard for general electrical applications, C10100 is strictly reserved for high-vacuum electronics and specialized welding where gas-free material is mandatory.
Why is the oxygen content in C11000 vs C10100 a deal-breaker for welding?
The oxygen in c11000 copper exists as cuprous oxide particles. If you attempt to weld or braze C11000 in a reducing atmosphere (containing hydrogen), the hydrogen diffuses into the copper and reacts with these oxides to form steam. This creates internal pressure that leads to hydrogen embrittlement and catastrophic cracking.
As detailed in our analysis of whether C11000 copper is oxygen free, C10100 eliminates this risk entirely because it is cast in a vacuum or inert gas environment. If your fabrication involves high-temperature processes, the choice between c11000 vs c10100 determines the structural integrity of the final assembly.
Comparative Chemical Limits (ASTM B152 / B170)
| Element | C11000 (ETP) | C10100 (OFE) |
| Copper (incl. Ag) | 99.90% Min | 99.99% Min |
| Oxygen (O) | 200 - 400 ppm | < 5 ppm |
| Lead (Pb) | 0.005% Max | 0.0005% Max |
| Sulfur (S) | 0.015% Max | 0.0015% Max |
| Total Impurities | Trace | < 100 ppm total |
Does 99.99% purity (C10100) actually improve electrical performance over 99.90% (C11000)?
In standard industrial applications, the difference is negligible. C11000 copper bar typically achieves 101% IACS conductivity, whereas C10100 reaches 101% to 102% IACS. The 1% gain is rarely worth the significant price increase for power distribution or C11000 copper bar used in standard busbars.
However, for high-vacuum applications or high-frequency electronics, the extreme purity of C10100 is necessary to prevent "outgassing" or signal loss. For a detailed breakdown of trace elements, consult the chemical composition of C11000 alloy. For common C11000 copper plate used in heat sinks, C11000 remains the preferred technical choice.
Physical and Mechanical Property Differences
| Property | C11000 (Half-Hard) | C10100 (Half-Hard) |
| Electrical Conductivity | 101% IACS | 101% - 102% IACS |
| Thermal Conductivity | 388 W/m·K | 391 W/m·K |
| Hardness | 65 - 95 HV | 65 - 95 HV |
| Elongation | ≥≥ 15% | ≥≥ 20% |
| Annealing Temp | 200°C - 350°C | 300°C - 600°C |
When is the C10100 price premium justified over standard C11000 copper?
Procurement managers must weigh the c11000 copper price against the technical requirements. C11000 is the most abundant and cost-effective grade (t2 copper) because it is produced via standard electrolytic refining. C10100 requires secondary induction melting in a vacuum, which can increase the cost by 20% to 50%.
The premium is justified only if:
The part will be welded or brazed at temperatures exceeding 400°C.
The material is used in ultra-high vacuum (UHV) systems.
You are manufacturing high-end audio components or specialized electronics requiring ultra-low noise.
For standard bending, punching, or CNC work, you can check the C110 copper bendable guide to see why C11000 is the standard for mechanical fabrication.
Get Real-Time Inventory Status
FAQ
1. Is C11000 a "Pure Copper"?
Yes. Any copper with a purity ≥ 99.90% is classified as commercially pure copper. Both C11000 and C10100 fall into this category despite the difference in refining levels.
2. Why is C11000 more popular for busbars than C10100?
Cost and availability. C11000 electrical copper busbar provides the exact same conductivity for power distribution systems as C10100 but at a much lower c11000 copper price.
3. Can I substitute C10100 with C10200?
Often, yes. C10200 is "Oxygen-Free" (OF) with 99.95% purity, while C10100 is "Oxygen-Free Electronic" (OFE) with 99.99% purity. Both solve the hydrogen embrittlement problem.
4. How do I verify if I received C10100 and not C11000?
Since they look identical, you must perform a chemical assay or an oxygen test. A simpler "hydrogen bend test" can be done by heating the sample in hydrogen; C11000 will fail the bend test, whereas C10100 will remain ductile.
5. Does C10100 machine better than C11000?
Actually, C11000 has a slight edge in machinability. The internal oxides help break the chips, whereas high-purity C10100 is "gummier" and can be harder to achieve a fine surface finish on custom cut C11000 copper plate.
6. Which grade is better for transformer coils?
Transformer C11000 copper coil is the industry standard. C10100 offers no functional benefit in oil-filled or dry-type transformers where high-heat welding is not required.
Product Specifications & Range
| Product Category | Common Grades (Alloys) | Size Range (Dimensions) | Standards |
| Copper Rods | C11000, C12200, C10200, C14500 | Diameter: 3mm – 400mm<br>Shape: Round, Hexagonal, Square | ASTM B187, EN 12163 |
| Copper Tubes | C11000, C12200 (DHP), C10200 (OF), C27200 | OD: 2mm – 219mm<br>Wall Thickness: 0.2mm – 20mm | ASTM B280, EN 12735 |
| Copper Plates | C11000 (ETP), C10200, C12200 | Thickness: 0.1mm – 150mm<br>Width: Up to 2500mm | ASTM B152, DIN 1751 |
| Copper Wires | C11000, C10200, Brass Wire | Diameter: 0.05mm – 10.0mm<br>Form: Spool or Coil | ASTM B3, EN 13602 |
| Copper Strips | C11000, C12200, C26800 (Brass) | Thickness: 0.05mm – 3.0mm<br>Width: 5mm – 610mm | ASTM B19, EN 1652 |
Customization Note:
Custom Dimensions: We provide precision cutting and slitting services to meet your specific project requirements.
Tempers Available: Soft (O), Half-Hard (H02), Full Hard (H04), and Spring Hard (H08).
Surface Finish: Bright annealing, Polished, or Plated (Tin, Silver, Nickel) upon request.
Industrial-Grade Export Packaging
Maximum protection against oxidation, moisture, and transit damage.
1. Anti-Oxidation Protection
VCI Paper & Moisture-Proof Film: Every order is vacuum-sealed or wrapped in anti-corrosion materials to ensure the copper remains bright and tarnish-free during sea freight.
2. Reinforced Structural Support
Seaworthy Wooden Crates: We use reinforced, fumigation-free wooden cases (ISPM-15) and steel strapping for rods, tubes, and heavy plates to prevent bending or surface scratches.
3. Secure Handling & Loading
Forklift-Ready Pallets: All materials are secured on standardized export pallets for easy unloading and maximum stability in containers.
4. Clear Identification
Professional Labeling: Each package includes detailed labels with heat numbers, specifications, and net weight for efficient inventory management.





Advanced Manufacturing & Quality Control
1. Core Production Equipment
Up-casting & Continuous Casting Lines: Ensures high-purity oxygen-free copper rods and wires with uniform grain structure.
High-Precision Cold/Hot Rolling Mills: Automated thickness control for copper plates and strips with tolerances within ±0.01mm.
Large-Scale Extrusion & Drawing Machines: Capable of producing seamless copper tubes and rods in diverse diameters and shapes.
Atmospheric Controlled Annealing Furnaces: Bright annealing process to achieve specific tempers (Soft, Half-hard, Hard) without surface oxidation.
2. In-House Testing Center
Direct-Reading Spectrometers: Instant chemical composition analysis to guarantee Cu purity and precise alloying (Brass, Bronze, etc.).
Universal Tensile Testers: Verifying mechanical properties including tensile strength, elongation, and yield strength.
Eddy Current & Ultrasonic Testing: 100% non-destructive inspection for tubes and rods to detect internal cracks or flaws.
Conductivity & Hardness Testers: Ensuring electrical conductivity (IACS) and Vickers/Rockwell hardness meet international standards (ASTM, EN, DIN).





Get Fast Quote & Logistics Plan