Introduction
This article explains C72200 copper-nickel-chromium alloy for seawater and chemical media service. C72200 is a copper-nickel-chromium alloy with about 15 to 18 percent nickel and a small chromium addition. It was developed for heat exchanger tubing in seawater and chemical service where higher strength and better resistance to high-velocity flow are required.
Composition
C72200 contains 15.0 to 18.0 percent nickel, 0.30 to 0.70 percent chromium and 0.5 to 1.0 percent iron with the balance copper. The chromium addition strengthens the alloy and improves the stability of the protective surface film, so the material resists erosion-corrosion and impingement attack better than the plain copper-nickel grades.
Corrosion Behavior
Like other copper-nickel alloys, C72200 forms a protective film in seawater that self-heals when damaged. The chromium-modified film is more resistant to high-velocity flow and to polluted water conditions, and the alloy shows good resistance to pitting, crevice attack and stress-corrosion cracking.
| Element | Typical Range |
|---|---|
| Nickel | 15.0 - 18.0% |
| Chromium | 0.30 - 0.70% |
| Iron | 0.5 - 1.0% |
| Copper | Balance |
Properties
The alloy reaches tensile strengths of about 380 to 450 MPa annealed with good ductility, and thermal conductivity of roughly 35 to 40 W/(m·K). It can be welded by standard processes and is available as seamless and welded tube, pipe, sheet and plate.
Applications and Standards
Typical uses are condenser and heat exchanger tubing in power plants, desalination units, chemical plants and offshore platforms, especially where cooling water velocities are high. The alloy is covered by standards such as ASTM B111, B122 and B171.
Verification
Confirm the nickel, chromium and iron ranges and the mechanical properties on the mill certificate, and check the tube dimensions and temper against the applicable standard before acceptance.