Identity of the Grade
C72200 is the UNS designation for a wrought copper-nickel alloy containing roughly 15-18 % nickel with a controlled chromium addition of 0.30-0.70 %. It is covered by the copper-nickel product specifications that also list C70400, C70600, C71000 and C71500, and it is produced in the same forms: seamless condenser and heat exchanger tube, seamless pipe and tube in straight lengths, plate sheet and strip, and rod and bar.
In Chinese trade usage the cupronickel family is often called white copper, and the term is applied loosely to both copper-nickel and copper-nickel-zinc alloys. For C72200 the accurate description is a chromium-bearing copper-nickel, sometimes written CuNi 85/15 Cr. It is not a copper-nickel-zinc alloy and it does not belong to the nickel silver group, whose members are defined by a substantial zinc content.
Chemical Composition
| Element | Content (wt %) | Contribution |
|---|---|---|
| Copper | Balance | Base metal, thermal conduction, ductility |
| Nickel, including cobalt | 15.0 - 18.0 | Corrosion resistance in seawater, solid-solution strengthening |
| Chromium | 0.30 - 0.70 | Strengthens the protective film, erosion-corrosion resistance |
| Iron and manganese | Within the limits set for the grade | Film stability and deoxidation |
| Lead | 0.05 max | Impurity control, weldability and cleanliness |
The element roles are worth reading together with the numbers. Nickel is the element that makes the alloy resistant to seawater; it is held in solid solution and also raises strength. Chromium is the element that makes the alloy different from the standard cupronickels, because it reinforces the surface film that protects the metal from flowing water. Iron assists in forming and stabilising that film, and manganese controls sulphur and oxygen during melting. Lead is restricted because it embrittles the alloy at hot working temperatures, harms weldability and is undesirable in any component that may come into contact with potable water.
Density and Physical Constants
The density of C72200 is typically in the range of 8.9 g/cm³, close to that of the 90/10 and 70/30 cupronickels, which all cluster around 8.9-8.94 g/cm³. The value is nearly the same across the family because nickel and copper have similar atomic masses, and it is useful in two practical contexts: mass estimation for a tube bundle or a pipe run, and identification of an unknown sample, since a piece of C72200 that weighs far less or far more than expected is not C72200.
| Property | Typical value |
|---|---|
| Density | Approximately 8.9 g/cm³ |
| Elastic modulus | Of the order of 140 - 150 GPa |
| Thermal conductivity at room temperature | Of the order of 30 W/(m·K) |
| Electrical conductivity | A few per cent IACS, far below pure copper |
| Magnetic behaviour | Essentially non-magnetic |
| Crystal structure | Single-phase face-centred cubic |
The low electrical and thermal conductivity compared with pure copper is a consequence of nickel in solid solution and is characteristic of the whole cupronickel family. It does not disqualify the alloy from heat exchanger service, because in a condenser the film resistance on the water and steam sides normally dominates the heat transfer path and the thin tube wall contributes little.
Impurity Limits and Why They Matter
The specification limits on lead, sulphur, phosphorus and carbon are not administrative detail. Sulphur and phosphorus must be kept low because they form brittle phases that reduce hot workability and can initiate cracking during welding. Carbon is restricted to avoid gas porosity in welds and in cast starting stock. Lead is limited for the reasons already given. A material certificate that reports only the major elements is therefore incomplete for a critical seawater application: the full chemical analysis, including residuals, is what confirms that the heat is genuinely to the specification.
Main Applications
Because the grade combines seawater corrosion resistance with resistance to erosion by suspended solids, the applications concentrate on cooling water duty: surface condenser and heat exchanger tube, seawater cooling pipework for ships and offshore installations, desalination heat transfer tube, tube plate and waterbox components, firewater and ballast systems, and heat exchangers in coastal power stations where the cooling water carries silt or sand. In each case the specification of C72200 over a standard cupronickel is a response to abrasive or high velocity water rather than a general preference.
FAQ
Q: What is the chemical composition of C72200?
Copper forms the balance with roughly 15-18 % nickel including cobalt and 0.30-0.70 % chromium, plus iron and manganese within the limits set for the grade and a maximum of 0.05 % lead.
Q: What is the density of C72200?
Approximately 8.9 g/cm³, essentially the same as the other wrought cupronickels, because copper and nickel have similar atomic masses.
Q: Is C72200 a nickel silver or white copper alloy?
The trade term white copper is applied to the copper-nickel family in Chinese usage, but C72200 is a chromium-bearing copper-nickel with no significant zinc content, and it is not a member of the nickel silver group.
Q: What is the grade used for?
Mainly condenser and heat exchanger tube and seawater cooling pipework where the water carries silt or sand and where the standard cupronickels would suffer erosion-corrosion.
Q: Why are impurity limits important in this grade?
Sulphur, phosphorus and carbon harm hot workability and weld quality, and lead embrittles the alloy during hot working and is undesirable in potable water service, so the residuals must be controlled and reported.
Q: Why is the alloy non-magnetic?
Its single-phase face-centred cubic structure is austenitic in character and carries no ferromagnetic phase, so the alloy is essentially non-magnetic in service.