What Is C72200 Cupronickel?
C72200 is the chromium-modified 85/15 copper-nickel alloy. Its base is the familiar cupronickel system, copper with roughly 15% nickel, and it is distinguished from the plain 90/10 and 70/30 alloys by a deliberate chromium addition together with controlled iron, manganese and titanium. That combination is what gives the alloy its specific reputation: it keeps the seawater corrosion resistance of a cupronickel while tolerating higher water velocities and more aggressive, chlorinated cooling water than the unmodified grades. Tubing made from it is used where impingement attack and erosion-corrosion, rather than general corrosion, set the limit of tube life.
Composition, Standards and Supplied Forms
Limits are fixed by the governing ASTM specification, and the alloy is supplied as seamless tube, welded and drawn tube, pipe, plate and sheet. The chromium level is small but critical to performance, and the iron, manganese and titanium additions assist film formation, hot ductility and castability respectively.
| Designation | Detail |
|---|---|
| UNS number | C72200 (CuNi 85/15 with chromium) |
| Nickel content | nominally about 15%, balanced copper |
| Chromium addition | small deliberate addition for erosion-corrosion resistance |
| Iron | added to stabilise the protective film |
| Seamless tube | ASTM B111/B111M, ASME SB111 |
| Seamless pipe | ASTM B466/B466M; welded pipe ASTM B467 |
| Plate and sheet | ASTM B171 and ASTM B122 families |
| Delivery condition | usually annealed and pickled |
Cold Working Behaviour
C72200 cupronickel cold works readily. The face-centred cubic structure gives good ductility at room temperature, so tube can be cold pilgered, cold drawn, rolled and bent without cracking provided the reduction per pass is matched to the available annealing capacity. In tube mills the sequence is normally: hot worked hollow, cold draw to an intermediate size, anneal to soften the cold-worked structure, pickle and lubricate, then continue drawing to the finished wall. The work hardening rate is moderate compared with a high-zinc brass, and the alloy tolerates the reductions needed to reach thin condenser walls with a limited number of passes.
Cold drawing and pilgering with inter-pass recrystallisation anneals
Bending and coiling in the annealed condition, with a stress relief anneal after severe cold forming
Good surface finish and dimensional control, important for thin-wall condenser tube
Finished tube is degreased and descaled after each anneal to prevent rolled-in oxide
Hot Working Behaviour
The alloy is hot worked in the upper part of its working range, where it is soft enough to extrude and pierce but still retains enough ductility to avoid edge cracking. In practice this means heating the billet uniformly, avoiding an overheated or locally burned surface, keeping the working time short and finishing above the temperature at which the structure becomes brittle. When hot working is completed, the material must not be left to cool slowly through the range where the iron and chromium-bearing phases can segregate; a rapid cool after the final hot pass, followed by a controlled anneal, is standard practice for producing a structure that will form a uniform protective film in service.
Hot working also gives the mill its opportunity to convert an as-cast ingot into a sound, fine-grained product. A properly hot worked and annealed C72200 tube has a uniform grain structure, which is exactly what the seawater film needs to develop evenly along the tube.
How Cold and Hot Working Are Combined in Tube Production
Modern condenser tube is not made by one process alone; the strength of the product comes from the sequence. A typical route for a C72200 tube is:
Melt and cast a controlled-composition billet with certified chemistry
Hot extrude or pierce into a hollow shell in the upper working range, then cool and condition the surface
Cold pilger and draw in several passes with intermediate anneals and pickles
Final anneal to the required temper so that the tube is soft enough to roll into the tube sheet
Straighten, cut to length, test by eddy current and hydrostatic pressure, and protect the ends for transport
Where C72200 Tube Is Used
The chromium addition pays for itself wherever the cooling water is fast, abrasive, chlorinated or full of suspended solids, and where a plain cupronickel tube would fail by impingement attack.
Steam condensers with high circulating-water velocity or high sand loading
Chlorinated seawater systems in power stations and desalination plant
Offshore cooling circuits, firewater systems and shipboard seawater services
Heat exchangers in refineries and chemical plant handling brackish and saline water
Marine and industrial piping where both erosion and corrosion are present
Ordering Guidance
To buy C72200 tube well, specify the UNS number, the governing standard and temper, the chemistry limits that matter for your water chemistry, the outside diameter and wall thickness with tolerances, length or U-bend geometry, the test schedule including eddy-current and hydrostatic tests, and the marking and protection requirements. It is also worth agreeing the acceptance criteria for grain size and surface finish, because a smooth internal bore and a uniform anneal are what allow the tube to form its protective film quickly and uniformly once it enters service.
Frequently Asked Questions
Q: Why does C72200 contain chromium?
The small chromium addition improves resistance to impingement attack and erosion-corrosion, which are the failure modes that limit plain cupronickel tubes in fast or solids-laden seawater.
Q: Is C72200 better than C70600 cupronickel?
For high-velocity, chlorinated or abrasive cooling water conditions it usually is, because it resists impingement attack better. For mild, slow seawater C70600 remains a lower-cost option.
Q: Can C72200 be cold worked without cracking?
Yes. The alloy has good room-temperature ductility and is cold drawn and bent in normal tube mill practice, with inter-pass anneals to remove work hardening and restore ductility.
Q: Can C72200 be hot worked?
Yes, but the billet must be heated uniformly, worked in the upper part of the working range and cooled rapidly afterwards, so that the chromium and iron bearing structure stays uniform.
Q: What temper is normally supplied for condenser service?
Condenser and heat exchanger tube is normally supplied annealed, so it is soft enough to be rolled into tube sheets and bent to U form without cracking.
Q: Does C72200 need special handling during installation?
Keep the tube clean and dry in storage, avoid dragging tools through the bore, and bring the cooling water on gradually so that the protective film forms before the tube meets its most aggressive service conditions.