Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
|
Density |
23.0 °C |
8.9 g/cm³ |
Typical for Wrought Copper Pure / Low Alloyed Copper |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
|
Elastic modulus |
23.0 °C |
95 - 98 GPa |
Typical for Wrought Copper Pure / Low Alloyed Copper |
|
Poisson's ratio |
23.0 °C |
0.34 [-] |
Typical for Wrought Copper Pure / Low Alloyed Copper |
|
Shear modulus |
23.0 °C |
48 GPa |
Typical for Wrought Copper Pure / Low Alloyed Copper |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
|
Coefficient of thermal expansion |
23.0 °C |
1.6E-5 - 1.8E-5 1/K |
Typical for Wrought Copper Pure / Low Alloyed Copper |
|
Melting point |
965 - 1100 °C |
Typical for Wrought Copper Pure / Low Alloyed Copper |
|
|
Specific heat capacity |
23.0 °C |
377 - 420 J/(kg·K) |
Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
| Property | Value |
|---|---|
|
Other |
Cu+Ag > 99.90 |
|
Phosphorus |
0.02 - 0.04 % |
|
Silver |
0.01 % |