What C12200 Copper Pipe Is
C12200 is phosphor-deoxidised copper, designated Cu-DHP in the European system, with a nominal copper content of 99.9% minimum including silver and a controlled phosphorus addition in the range 0.015 to 0.040%. The phosphorus is added deliberately, not left as a residue. It combines with oxygen during melting, so the cast material is free of cuprous oxide particles and the tube can be brazed or welded in hydrogen-bearing atmospheres without the embrittlement that affects the oxygen-bearing tough pitch grades.
The grade is the workhorse of water tube, refrigeration tube and general engineering tube. It is also known as CW024A in EN 1057, as C1220 in JIS H3300, as TP2 in GB/T 18033 and GB/T 17791, and as the deoxidised copper heat exchanger and condenser tube covered by ASTM B111 where seawater cooling is not severe enough to require an alloy grade.
Standards That Cover C12200 Pipe and Tube
| Standard | Product covered | Typical service |
|---|---|---|
| ASTM B88 | Seamless copper water tube, Types K, L, M | Potable water, heating and cooling systems |
| ASTM B75 / B75M | Seamless copper pipe and tube | General engineering, piping and process lines |
| ASTM B280 | Seamless copper tube for air conditioning and refrigeration | Refrigerant circuits and ACR coil |
| ASTM B111 | Seamless condenser tube and ferrule stock | Heat exchangers and condensers |
| ASTM B306 | Copper drainage tube, DWV | Above-ground sanitary and drainage work |
| EN 1057 | Seamless round copper tube for water and gas | Sanitary and heating installations |
| JIS H3300 | Copper and copper alloy seamless tube | Water, refrigeration and general service |
| GB/T 18033, GB/T 17791 | Seamless copper tube for water, refrigeration and air conditioning | Domestic and export projects |
Each standard controls a different combination of composition, dimensions, temper, mechanical properties and internal cleanliness, so the same nominal C12200 tube ordered to two different standards is not necessarily interchangeable. Air conditioning tube, for example, is held to tighter cleanness and moisture limits than general-purpose water tube, because its bore carries a refrigerant charge through a capillary restrictor.
Composition and Temper Control
| Element | Requirement, % |
|---|---|
| Cu, including Ag | 99.90 min |
| P | 0.015 - 0.040 |
| Other elements | Restricted by the individual standard to protect conductivity and formability |
The phosphorus window is deliberately narrow. Below the lower limit the deoxidation is incomplete and residual oxide particles remain in the structure; above the upper limit the conductivity of the metal falls noticeably, because dissolved phosphorus is a very effective scattering centre for electrons. That is why C12200 is specified where a combination of brazeability, formability and moderate conductivity is required, while the oxygen-free grades C10100 and C10200 are specified when the highest achievable conductivity is the deciding factor.
Temper governs the mechanical properties. The soft annealed condition is used for coiled tube and for bending on site, since it deforms easily without cracking. The drawn and hard tempers raise yield strength and pressure rating and are used for straight runs. Ordering to a standard without naming the temper leaves the most important single variable of the tube unspecified.
Interchangeable Grades
| System | Designation |
|---|---|
| UNS | C12200 |
| European designation | Cu-DHP, CW024A |
| Japanese | C1220 |
| Chinese | TP2 |
These designations describe the same deoxidised copper composition and can be used interchangeably in most water and refrigeration applications, provided the tube is ordered to the standard appropriate to the service and the dimensional tolerances match the fittings being used. Differences that do matter in practice are manufacturing origin, since EN 1057 requires wall thickness to be specified as a precise value with tight tolerance, while ASTM B88 is written around nominal wall thickness with a broader permitted range.
How to Specify and Verify C12200 Tube
Name the standard, the grade, the temper, the outside diameter, the wall thickness or wall type and the length.
State the test requirement: hardness for temper verification, eddy-current testing of the finished tube, hydrostatic test where pressure integrity is critical, and dimensional inspection of diameter, wall and eccentricity.
State the cleanliness requirement. Residual drawing lubricant and carbon film are the main causes of problems in refrigeration and heat exchanger service.
Require heat number traceability and a certificate of analysis where the tube will be welded or brazed into a structure with its own quality plan.
Confirm that end protection, marking and packaging suit ocean transport for export shipments.
FAQ
Q: What does the designation C12200 mean?
It is the UNS number for phosphor-deoxidised copper containing at least 99.90% copper including silver, with phosphorus between 0.015 and 0.040%. The same material appears as Cu-DHP and CW024A in Europe, C1220 in Japan and TP2 in China.
Q: Why is phosphorus added to copper tube?
Phosphorus removes oxygen from the melt so that no oxide particles remain in the metal. Tube made this way can be brazed without the risk of hydrogen embrittlement and behaves predictably in welded assemblies.
Q: What is the difference between C12200 and C11000?
C11000 is electrolytic tough pitch copper, which contains a small amount of oxygen and has the highest practical conductivity. C12200 is deoxidised with phosphorus, which slightly lowers conductivity but makes the material far more suitable for brazed and welded assemblies.
Q: Which standard applies to water tube versus refrigeration tube?
Water tube is normally ordered to ASTM B88 or EN 1057, while air conditioning and refrigeration coil is ordered to ASTM B280 or EN 12735. The refrigeration standards impose tighter limits on cleanness, moisture and wall uniformity to protect the refrigerant circuit.
Q: Does temper affect the pressure rating?
Yes. The drawn and hard tempers have higher yield strength and therefore a higher permitted working pressure at a given wall thickness than the annealed temper. Annealed tube is chosen where the tube must be bent or coiled on site.
Q: How should C12200 tube be inspected on delivery?
Check marking and heat number traceability against the certificate, measure outside diameter, wall thickness and roundness at several positions, verify temper by hardness or tensile test, and confirm surface and bore cleanliness. Eddy-current or hydrostatic testing is specified where the tube will operate under pressure in a critical circuit.