Sep 28, 2025 Leave a message

C37700 Brass Heat Exchanger Tube: CuZn38Pb2 Composition, Properties and Applications

What C37700 Brass Tube Is

UNS C37700 is a leaded brass of the CuZn38Pb2 family. Copper is held between 58% and 61%, with 1.5-2.5% lead distributed through the matrix and zinc forming the balance. The lower copper level compared with other brass tube grades reduces raw material cost, while the lead dispersion keeps chips short during machining and lubricates the die during hot forming. The alloy is covered by ASTM B453 for leaded brass rod and bar, by ASTM B121 for leaded brass plate, sheet, strip and rolled bar, and by SAE J463 for wrought copper and copper alloy products.

Tube in this grade is supplied in the bright condition, meaning it leaves the final drawing or annealing step with a clean, oxide-free surface suitable for plating, lacquering or direct assembly. Hot forming is carried out in the 700-800 C window, where the alpha-beta structure of the alloy is sufficiently ductile for extrusion, upsetting and pressing of fittings, water box stubs and radiator components.

Chemical Composition and Standards

Element Weight % Notes
Copper (Cu) 58-61 Controls cost balance and corrosion behaviour
Zinc (Zn) Balance Principal alloying element
Lead (Pb) 1.5-2.5 Machinability and chip control
Iron (Fe) 0.30 max Residual; higher tolerance than C34200
Other impurities 0.80 max total Sum of unspecified elements

Note that the wider residual allowances, compared with a tube-grade brass such as C34200, make C37700 more tolerant of recycled charge material and therefore more economical in high-volume production. The trade-off is a slightly lower corrosion resistance and a somewhat broader property scatter, which is why the grade is not selected for critical seawater-wetted heat transfer surfaces.

Physical and Mechanical Properties

Density lies in the range 8.44-8.53 g/cm³ and the melting range is 895-940 C. Thermal conductivity is about 121 W/m.K at 20 C, and electrical conductivity is 24-27% IACS in the annealed condition. The comparatively high thermal conductivity supports the use of the alloy in radiator and cooler tubing where heat must cross the tube wall quickly.

Condition Tensile strength (MPa) Yield strength (MPa) Elongation (%) Hardness (HV)
Annealed (soft) 260-440 100-200 35-50 75-100
Cold worked (H02) 450-550 350-450 15-25 120-160
Hard (H04) 550 min 450 min 5 min 160 min

Product forms available in this grade include tube from 10 mm to 250 mm outside diameter with 1.0 mm to 15.0 mm wall, rod and bar from 3 mm to 150 mm, strip 0.3 mm to 6.0 mm thick and wire from 0.5 mm to 12 mm.

Applications

Heat exchanger and cooler tubing: inner tubes, return bends, radiator cores and layer-wound coil stock.

Automotive: radiator and heater cores, fuel system parts and stamped components produced at high volume.

Plumbing hardware: low-pressure fittings, valve bodies, couplings and adapters.

Electrical and electronic hardware: connectors, terminals and shielding parts.

General mechanical parts: gears, bushings and fasteners made from bar or heavy-wall tube.

Hot forming is a particular strength of the grade. Forgings, pressings and extruded profiles can be produced from heated stock with good die fill and low forming loads, which suits the production of fittings and header components that are subsequently joined to tube.

Bright Finishing, Welding and Selection Notes

Bright finish. The bright surface is produced by controlled drawing lubricants and reducing or protective atmospheres during annealing. Store tube with end caps in a dry place and handle with gloves; the finished surface should not be abraded before plating or lacquering.

Annealing. Soften at 600-650 C for 1-2 hours to restore ductility after cold drawing, then cool in a protective atmosphere to preserve the bright surface.

Machining. Use sharp carbide tooling with adequate lubricant and chip clearance; the lead content keeps cutting forces low, but excessive speed raises edge temperature and smears the surface.

Welding and brazing. Brazing and soldering are the preferred joining processes. When fusion welding is used, keep heat input low, shield with inert gas and provide fume extraction so that the volatile lead phase does not contaminate the weld pool.

Corrosion limits. The alloy resists atmosphere and fresh water but is not intended for continuous saltwater or ammonia-rich service. Where seawater corrosion resistance is required, an inhibited tube alloy should be selected and the wetted surfaces protected accordingly.

Inspection. Confirm wall thickness by ultrasonic or mechanical gauging, check concentricity on drawn tube, and request a mill test certificate covering chemical analysis and the mechanical results for the delivered temper.

FAQ

Q: Why choose C37700 rather than a higher-copper brass tube?
The lower copper range of 58-61% reduces material cost and the alloy remains easy to machine and hot form. It is the economical choice for high-volume automotive and hardware parts where seawater-grade corrosion resistance is not needed.

Q: What does bright tube mean in practice?
The tube is delivered with a clean, oxide-free surface produced by controlled drawing and protective-atmosphere annealing, so it can be plated, lacquered or assembled without a pickling step.

Q: Is C37700 suitable for hot forging?
Yes. Its alpha-beta structure gives good ductility above roughly 700 C, which allows extrusion, pressing and upsetting of fittings and header parts with good die fill and moderate forming loads.

Q: How should tube expanding be carried out?
Use annealed tube for roller expanding or flaring, lubricate the expander, and advance it in stages so that the wall is not stretched beyond the elongation available in the ordered temper.

Q: What are the main risks during fusion welding?
Overheating volatilises part of the lead phase, producing fume and a porous weld. Keep the heat input low, use inert gas shielding, provide local extraction and design the joint so most of the length is brazed rather than welded.

Q: Which documents accompany an export shipment?
A mill test certificate with chemical and mechanical results, a dimensional report on request, and a packing list describing seaworthy export packaging. Third-party inspection can be arranged when the buyer nominates an agency.

Send Inquiry

whatsapp

Phone

E-mail