Scope of ASTM B152 and the C10100 Grade
ASTM B152/B152M covers copper sheet, strip, plate and rolled bar in the wrought, mill-product forms. It is a flat-rolled and rolled-bar specification: it defines the plate and strip used for tube sheets, baffles, gaskets, busbars, vacuum chamber walls and formed components. Tube forms - including the condenser and heat-exchanger tubes used in the same assemblies - are ordered to the tube specifications instead, most commonly ASTM B111/B111M for condenser tubes and ASTM B88/B88M or B75 for water tube and pipe. When a project requires a condenser bundle and its tube sheet, both documents apply simultaneously, and the C10100 grade is the grade that ties them together.
UNS C10100 is the oxygen-free electronic grade. It is the highest-purity copper in general industrial supply, and its defining feature is not only the copper content but the extremely low oxygen level, which removes the risk of hydrogen embrittlement during brazing, welding or high-temperature processing.
Chemical Composition and Purity
| Element | Requirement |
|---|---|
| Copper, Cu (including silver) | 99.99% min |
| Oxygen, O | 0.0005% max |
| Remaining elements | Total limited to the trace levels of the specification |
The oxygen limit is the reason this grade exists. In ordinary electrolytic tough pitch copper, oxygen is present as copper oxide particles; in a hydrogen-bearing atmosphere at elevated temperature those particles react and generate steam, which opens up grain boundaries and cracks the metal. C10100 removes that mechanism, which is why it is the grade chosen for electron tubes, vacuum seals and glass-to-metal components that must survive a hydrogen firing step.
Physical Properties
| Property | Metric | Imperial |
|---|---|---|
| Density | 8.89 - 8.94 g/cm³ | 0.321 - 0.323 lb/in³ |
| Melting point | 1083 C | 1981 F |
| Modulus of elasticity | 115 GPa | 16700 ksi |
| Poisson's ratio | 0.31 | 0.31 |
| Electrical conductivity | Above 100% IACS | Above 100% IACS |
The combination of very high electrical and thermal conductivity with high ductility is what makes the light annealed temper so useful in heat transfer and power applications: heat passes through the wall quickly, and the metal accommodates thermal expansion and formed joints without cracking.
Temper Selection: Light Annealed and Harder Tempers
ASTM B152 defines a range of tempers from soft annealed through to hard rolled. The light annealed condition is a soft, fully recrystallised temper: strength is at the low end of the range and elongation at the high end. That balance matters in formed parts, where the material has to be bent, flanged, spun or deep drawn without splitting.
| Condition | Strength level | Formability | Typical use |
|---|---|---|---|
| Light annealed / soft anneal | Lowest of the temper range | Highest ductility | Deep drawn parts, gaskets, formed shells, gasket rings |
| Half hard | Intermediate | Moderate | Busbars, plates requiring stiffness |
| Full hard | Highest of the range | Low | Springs, strip contacts, wear-resistant liners |
For sheet and strip in this grade, tensile strength rises from roughly 221 MPa in the softest condition up to about 455 MPa in the hardest, and yield strength varies over a still wider band, because the temper rather than the chemistry controls the level. That is why a purchase enquiry based only on chemistry is incomplete: the temper designation is what fixes the mechanical result.
Applications
Vacuum equipment, electron tubes, waveguides and glass-to-metal seals where hydrogen firing is used.
High-conductivity conductors, transformer windings and busbar components in electrical engineering.
Heat exchange elements, condenser-related components and vacuum coating equipment, where thermal conductivity dominates the design.
Gaskets, gasket rings, baffles and tube sheets in heat transfer assemblies.
Precision strip parts such as lead frames and shielding components.
Common Pitfalls and Inspection Points
Ordering a "condenser tube" against a flat-rolled specification. Tube, pipe, sheet and plate are covered by different documents; check that the mill certificate names the correct product form as well as the correct grade.
Specifying C10100 where C11000 would do, or the reverse. If the part will be brazed or fired in hydrogen, the oxygen-free grade is essential; where it will not, C11000 is usually more economical and equally conductive.
Ignoring temper on the purchase order. Chemistry alone will not reproduce the forming behaviour of the original part.
Surface contamination from handling. Copper picks up fingerprints and sulfur compounds readily; protective film or paper interleaving should be requested for critical surfaces.
Inspection normally covers chemical analysis, tensile test, grain size in the annealed condition, dimensional checking and, for electrical duty, conductivity verification.
FAQ
Q: Is C10100 the same as C10200?
Both are oxygen-free coppers with very low oxygen, and both are hydrogen-resistant. C10100 is the electronic grade with a 99.99% minimum copper content, while C10200 is specified at a lower minimum copper content. C10100 is chosen where the highest conductivity and purity are required; C10200 covers the majority of general oxygen-free duty at lower cost.
Q: Why does a condenser tube enquiry sometimes reference B152?
Because the same assembly contains both flat-rolled and tubular products. The tube sheets, baffles and gaskets in a condenser are flat-rolled items covered by ASTM B152, while the tubes themselves are covered by ASTM B111 or the water tube specifications. Both documents are normally cited on a single project specification.
Q: What does light annealed actually mean in practice?
It describes the softest usable mill temper, produced by annealing after rolling so that the grain structure is fully recrystallised. The result is the lowest strength and the highest elongation available in the grade, which is what formed and drawn components need. The temper designation on the certificate is the only reliable way to confirm it.
Q: Can C10100 be welded?
Yes, and its low oxygen content makes it far more forgiving than tough pitch copper. Welding still requires high heat input, preheating for thicker sections and careful joint cleaning, because copper conducts heat away so quickly that lack of fusion is the usual defect rather than cracking.
Q: How is conductivity verified?
Conductivity is normally confirmed against the specification requirement using an electrical resistivity measurement on a prepared specimen, expressed as a percentage of the International Annealed Copper Standard. Conductivity is reported alongside the chemical certificate for electrical applications.