Sep 25, 2025 Leave a message

ASTM B111 C12200 Thin Wall Copper Tube for Heat Transfer Equipment

Thin wall copper tube produced to ASTM B111 in UNS C12200 is the workhorse material of steam-to-water and water-to-air heat transfer. C12200 is phosphorus-deoxidized copper, commonly described as DHP copper, in which residual phosphorus is deliberately retained within a controlled range. Deoxidation removes the oxygen that would otherwise form cuprous oxide at grain boundaries and embrittle the metal during brazing or welding, so thin wall tube can be bent, expanded and joined without cracking.

Because thin wall tubing is chosen where heat transfer surface and equipment weight are both optimised, C12200 combines very high thermal conductivity with the ductility needed for U-bends, coils and rolled tube-to-tubesheet joints. It performs well in fresh water, steam condensate and many neutral process fluids, which is why deoxidized copper remains the reference material for transferring heat from steam to water or air.

Material Definition and Applicable Standards

ASTM B111/B111M covers seamless tube and ferrule stock of copper and copper alloys up to 3 1/8 in. (80 mm) inclusive in diameter for surface condensers, evaporators and heat exchangers; C12200 is the deoxidized copper grade listed in that specification.

ASME SB111 applies the same requirements where pressure-equipment acceptance is required.

EN 12451 and the EN 1412 designation Cu-DHP, material number CW024A, describe the European equivalent of the same deoxidized copper.

GB/T 8890 and JIS H3300 cover seamless copper tubes for heat exchanger service in the Chinese and Japanese systems.

Common delivery tempers are annealed (O61 or O60) for bending, coiling and rolling into tubesheets, and light drawn for straight lengths that must stay straight.

Chemical Composition of C12200 DHP Copper

Element Requirement Function
Cu + Ag 99.90 % min Base metal; silver counts with copper
P 0.015 - 0.040 % Deoxidation; controls residual oxygen
Other elements Within the limits stated in ASTM B111 Keeps the alloy within the deoxidized copper grade

The specified phosphorus range is the defining feature of C12200: it is what separates DHP copper from the oxygen-free grades and from electrolytic tough pitch copper, which still contains oxygen and is unsuitable for welding or hydrogen-bearing service.

Mechanical Properties, Physical Data and Dimensions

Thermal conductivity is approximately 339 W/(m·K) at room temperature, one of the highest values available in a heat exchanger tube material.

Tensile strength and yield strength are taken from the alloy and temper tables of ASTM B111; the tube is tension tested to ASTM E8/E8M with elongation measured over 50 mm in the annealed temper.

Annealed tube is supplied with a controlled nominal grain size that is verified metallographically, which governs bendability and the quality of expanded joints.

Acceptance tests include expansion of the tube outside diameter, flattening, eddy current examination to ASTM E309 and a hydrostatic or pneumatic test as ordered.

Outside diameter and wall thickness follow the standard size tables, with thin wall denoting walls at the lower end of the range while still leaving enough metal for pressure retention and for rolling into a tubesheet.

Tube is supplied in straight lengths, as U-bent hairpins or coiled, with plain or prepared ends depending on the joining method.

Applications

Sugar refinery condensers, evaporators and juice heaters, where the tube is exposed to steam and condensate.

Power plant surface condensers and feedwater heaters using clean fresh water or treated cooling water.

Distiller, brewery and dairy heat exchangers, including steam-to-water exchangers and hot water generators.

HVAC and refrigeration condensers, evaporators and air coolers, including finned coil assemblies.

Solar thermal absorbers, flat plate collectors and other conduction equipment where high thermal conductivity matters more than strength.

Selection, Fabrication and Installation Guidance

Size the tube on both sides of the wall: steam-side condensing performance is dominated by thermal resistance, while water-side velocity must stay inside the range set by the exchanger designer. Excessive velocity promotes erosion, and very low velocity encourages deposits.

For brazed joints, copper tubing can be joined with phosphorus-bearing copper filler alloys that do not need flux; use a controlled atmosphere or flux appropriate to the filler for silver brazing.

Where tube is expanded into a tubesheet, keep the annealed temper and control expansion so that wall reduction stays within the joint design; over-rolling work hardens the metal and can cause longitudinal cracking.

Stress relieve tube that will see ammonia or ammonium-bearing environments, because copper alloys are susceptible to stress corrosion cracking in those media.

Support and baffle the bundle so that flow-induced vibration does not cause fatigue at the tubesheet.

Inspection Points and Common Pitfalls

Confirm that the certificate states C12200 with the phosphorus range, not simply copper, since C11000 tough pitch copper will not weld or tolerate hydrogen-bearing service.

Verify eddy current and hydrostatic test records against the order; thin wall tube has little corrosion allowance, so an undetected longitudinal defect is critical.

Check ovality and wall eccentricity, which directly affect expansion joints and heat transfer uniformity.

Keep tube ends capped and dry in storage; acetic-acid attack from packaging materials causes bright, shallow corrosion that shows up only after installation.

Do not mix C12200 with admiralty or copper-nickel tubes in the same seawater bundle without considering galvanic effects at the tubesheet.

FAQ

Q: What does the C12200 designation mean?
C12200 is the UNS number for phosphorus-deoxidized copper, also written Cu-DHP or CW024A. It contains at least 99.90 % copper plus silver and 0.015 to 0.040 % phosphorus.

Q: Why is deoxidized copper preferred over tough pitch copper for heat transfer tube?
Deoxidation removes oxygen, so the metal can be brazed, welded and bent without grain-boundary embrittlement. Tough pitch copper contains oxygen and is not suitable for those operations.

Q: What wall thickness counts as thin wall?
Thin wall normally means a wall thickness at the lower end of the sizes listed in ASTM B111 for the stated outside diameter. The wall must still satisfy the working pressure, the expansion joint design and the expected corrosion allowance.

Q: Which tempers are used for C12200 heat transfer tube?
Annealed temper, designated O61 or O60, is used where the tube is bent, coiled or rolled into a tubesheet. A light drawn temper is chosen for straight runs that must remain straight and stiff.

Q: How is C12200 tube tested before shipment?
Requirements include tension testing to ASTM E8/E8M, grain size verification on annealed tube, expansion and flattening tests, eddy current examination to ASTM E309 and a hydrostatic test as specified on the purchase order.

Q: Can thin wall C12200 tube be used in seawater?
It performs well in fresh water and condensate but is not the preferred choice for flowing seawater, where admiralty brass or copper-nickel grades with higher resistance to erosion and impingement are normally selected.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry